Mar 4, 2001 #1 lcl Mechanical Joined May 24, 2005 Messages 2 Location MX Any information on corrosion rates for forged Nickel-Aluminium Bronze in sea water at up to 4m/s.
Mar 14, 2001 #2 rustbuster Petroleum Joined Jul 7, 1999 Messages 289 Corrosion rate in quiet sea water is 1 - 2 mpy. Check the NACE site, they should have more info. (http://www.nace.org) Upvote 0 Downvote
Corrosion rate in quiet sea water is 1 - 2 mpy. Check the NACE site, they should have more info. (http://www.nace.org)