Oct 29, 2011 #1 zanbaq Materials Joined Oct 10, 2011 Messages 26 Location US what is corrosion rate of carbon steel vessel where water flow slowly?
Oct 29, 2011 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Impossible to answer because there is not enough information. Information needed; 1. Water quality or type of water 2. Temperature 3. Flow rate Upvote 0 Downvote
Impossible to answer because there is not enough information. Information needed; 1. Water quality or type of water 2. Temperature 3. Flow rate
Oct 29, 2011 Thread starter #3 zanbaq Materials Joined Oct 10, 2011 Messages 26 Location US thank you Metengr Is there any reference that get me corrosion rate of carbon steel in diffrent situation? Upvote 0 Downvote
thank you Metengr Is there any reference that get me corrosion rate of carbon steel in diffrent situation?
Oct 30, 2011 Thread starter #4 zanbaq Materials Joined Oct 10, 2011 Messages 26 Location US temperature:ambient temperaturere conduct of water: 62 pH: 7.2 flow rate: 200 m3/h Upvote 0 Downvote
Oct 30, 2011 1 #5 SJones Petroleum Joined Apr 22, 2001 Messages 3,946 Location GB Google the following: "Corrosion Survey Database - COR-SUR" Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04 Upvote 0 Downvote
Google the following: "Corrosion Survey Database - COR-SUR" Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04
Oct 31, 2011 #6 mrfailure Materials Joined Aug 7, 2011 Messages 817 Location US Look in The Handbook of Corrosion Data from ASM, which reports corrosion rate test data from lots of sources under varying conditions. Aaron Tanzer http://www.lehightesting.com Upvote 0 Downvote
Look in The Handbook of Corrosion Data from ASM, which reports corrosion rate test data from lots of sources under varying conditions. Aaron Tanzer http://www.lehightesting.com