what is corrosion rate of carbon steel vessel where water flow slowly?
 
Impossible to answer because there is not enough information.

Information needed;

1. Water quality or type of water
2. Temperature
3. Flow rate
 
thank you Metengr
Is there any reference that get me corrosion rate of carbon steel in diffrent situation?
 
temperature:ambient temperaturere
conduct of water: 62
pH: 7.2
flow rate: 200 m3/h
 