Aug 4, 2010 #1 engrom Materials Joined Jul 31, 2003 Messages 92 Location AU Can anyone give estimate figures for corrosion rate of unprotected carbon steel in seawater as a factor of depth and temperature? Are there any technical literature/study reports which is useful? Thanks
Can anyone give estimate figures for corrosion rate of unprotected carbon steel in seawater as a factor of depth and temperature? Are there any technical literature/study reports which is useful? Thanks
Aug 4, 2010 #2 SJones Petroleum Joined Apr 22, 2001 Messages 3,950 Location GB There are a whole series of papers in Corrosion by R E Melchers one of which is: Effect Of Immersion Depth On Marine Corrosion Of Mild Steel Vol 61, (9), 2005, pp 895-906 there are other for temperature, water velocity, nutrient content and many more parameters Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04 Upvote 0 Downvote
There are a whole series of papers in Corrosion by R E Melchers one of which is: Effect Of Immersion Depth On Marine Corrosion Of Mild Steel Vol 61, (9), 2005, pp 895-906 there are other for temperature, water velocity, nutrient content and many more parameters Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04
Aug 5, 2010 Thread starter #3 engrom Materials Joined Jul 31, 2003 Messages 92 Location AU Thanks Steve for this valuable tip. Upvote 0 Downvote
Aug 5, 2010 1 #4 strider6 Materials Joined May 4, 2007 Messages 616 Location IT i suggest u also this paper: http://www.dtic.mil/cgi-bin/GetTRDoc?AD=AD820155&Location=U2&doc=GetTRDoc.pdf http://www.corrosionist.com/Corrosion_Control_Seawater.htm it contains a lot of info on sea water corrosion and on the effect of th emain factors like salt content, oxygen content.. hope this help S Corrosion & Rust Prevention Control Upvote 0 Downvote
i suggest u also this paper: http://www.dtic.mil/cgi-bin/GetTRDoc?AD=AD820155&Location=U2&doc=GetTRDoc.pdf http://www.corrosionist.com/Corrosion_Control_Seawater.htm it contains a lot of info on sea water corrosion and on the effect of th emain factors like salt content, oxygen content.. hope this help S Corrosion & Rust Prevention Control