corrosion protection for cad plated repairs

Status
Not open for further replies.

sigma38

Aerospace
Joined
Apr 10, 2007
Messages
25
Location
US
For small areas of cad plating that have worn, or been machined, off of steel and nickel-aluminum-bronze (e.g. bushings), what are folks seeing done to protect the surface without having to re-cad plate?
 
Could you tell us more about "brush cadmium plating"? Do you have material and application specification references by chance?

Thanks.
 
Actually, let me adjsut the question... a quick google brought up a lot of info... what spec seems to be the aero industry standard for this process?
 
The Iridite made the US Navy happy for ship-board stuff back in the days when I was building stuff for the Navy.
 
Standards:

AMS 2451/4B --Plating, Brush, Cadmium Corrosion Protective, Low Hydrogen Embrittlement

AMS-QQ-P-416 --Plating, Cadmium (Electrodeposited)
 
MIL-STD-865D Selective Brush Plating, Electro-Deposition

Regards, Wil Taylor
 