Dec 18, 2008 #1 sigma38 Aerospace Joined Apr 10, 2007 Messages 25 Location US For small areas of cad plating that have worn, or been machined, off of steel and nickel-aluminum-bronze (e.g. bushings), what are folks seeing done to protect the surface without having to re-cad plate?
For small areas of cad plating that have worn, or been machined, off of steel and nickel-aluminum-bronze (e.g. bushings), what are folks seeing done to protect the surface without having to re-cad plate?
Dec 18, 2008 #2 M MintJulep Mechanical Joined Jun 12, 2003 Messages 10,251 Location JP Iridite http://galladechem.com/specs/macdermid/78650.pdf Upvote 0 Downvote
Dec 19, 2008 #3 swall Materials Joined Sep 30, 2003 Messages 2,767 Location US Brush cadmium plating. Upvote 0 Downvote
Dec 19, 2008 Thread starter #4 sigma38 Aerospace Joined Apr 10, 2007 Messages 25 Location US Could you tell us more about "brush cadmium plating"? Do you have material and application specification references by chance? Thanks. Upvote 0 Downvote
Could you tell us more about "brush cadmium plating"? Do you have material and application specification references by chance? Thanks.
Dec 19, 2008 Thread starter #5 sigma38 Aerospace Joined Apr 10, 2007 Messages 25 Location US Actually, let me adjsut the question... a quick google brought up a lot of info... what spec seems to be the aero industry standard for this process? Upvote 0 Downvote
Actually, let me adjsut the question... a quick google brought up a lot of info... what spec seems to be the aero industry standard for this process?
Dec 19, 2008 #6 M MintJulep Mechanical Joined Jun 12, 2003 Messages 10,251 Location JP The Iridite made the US Navy happy for ship-board stuff back in the days when I was building stuff for the Navy. Upvote 0 Downvote
The Iridite made the US Navy happy for ship-board stuff back in the days when I was building stuff for the Navy.
Dec 20, 2008 #7 Flesh Materials Joined Jul 17, 2003 Messages 108 Location US Standards: AMS 2451/4B --Plating, Brush, Cadmium Corrosion Protective, Low Hydrogen Embrittlement AMS-QQ-P-416 --Plating, Cadmium (Electrodeposited) Upvote 0 Downvote
Standards: AMS 2451/4B --Plating, Brush, Cadmium Corrosion Protective, Low Hydrogen Embrittlement AMS-QQ-P-416 --Plating, Cadmium (Electrodeposited)
Dec 30, 2008 #8 WKTaylor Well-known member Joined Sep 24, 2001 Messages 4,318 Location US MIL-STD-865D Selective Brush Plating, Electro-Deposition Regards, Wil Taylor Upvote 0 Downvote