jsobilo1354
Mechanical
- Aug 9, 2006
- 11
I am seeing significant corrosion rates (.020"/yr.) on A249 TP316L HT tubes (.750",.060" AW) in rich amine service (CO removal). These shell and tube heat exchangers were replaced 3 years ago(in-kind). The previous exchangers were in service a little over 10 years. I have pulled samples and in the process of completing metallurgical examinations. I have also sampled tubes with eddy-current but was only able to inspect a small portion of the entire length of the tube due to a hard, tight black corrosion product that could not be removed(10,000 psi hydroblasting could not remove this scale completly). The areas that could be tested revealed 50%-60% wall loss from nominal "t".
Has anyone seen these type corrosion rates in this service with this type SS?