Could anybody inform about corrosion inhibitors for products, gas transport cross country pipelines.You may also directly reply at caltech@vsnl.net
 
Replies continue below

Recommended for you

What are the properties of VCI. What are benifits and type of protections it can give. Could you please clarify.
 
VCI's will not be appropriate for operating pipelines. Their principal use would be for preservation. You need to look at some specialist chemical suppliers' web sites. Try:

Steve Jones
Shell Iran Offshore Ltd, Dubai
 
Suggest you contact Nalco. They are owned by Ondeo now. Sharing knowledge is a way to immortality
 
VCIs are originaly developed to protect boilers and piping systems of ships to be mothballed, the volatile corrosion inhibitor(VCI)has been modified over the years to protect electronics, pacaged items,reinforced concrete, coated metaland mateal working fluids. VCIs are powerful tool in combatting atmospheric corrosion of metal and alloys. Because they are volatile at ambient temperature, VCI compounds can reach inaccessible crevices in metallic structures.Protective vapors disseminate within an enclosed space until reaching equilibrium,which is determined by the partial vapor pressure of the VCI compound.The inhibiting process starts when the vapours contact the metal surface and condense to form a thin film of microcrystals. In the presence of even minute quantities of moisture, the crystals dissolve and develop strong ionic activity. Ad sorption of mixed VCI compounds changes the energy state of metallic ions on the surface, diminishing the tendency of metal to ionized and dissolve.
 