Corrosion inhibitor and flow pressure

Status
Not open for further replies.

hamdykhalaf

Materials
Feb 14, 2015
6
the pipeline is recieving a constant dosing rate of Corrosion inhibitor , the production team are requiring to reduce the flow pressure , is there any necessity to change the CI dosing rate ?
 
Replies continue below

Recommended for you

It depends on what basis the dosing rate has been established and whether that basis is altered by the reduction in system pressure.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
The corrosion inhibitor feed rate should be proportional to flow.

If the CI feed pump is constant speed, you may dilute the mixture to reduce the CI rate of flow.
 
Typically yes, the corrosion inhibitor is probably calculated to production rate, or in turn the amount of water being transported down the line
 