I work at a nickel concentrator and I am in the process of replacing several componets in my thickeners due to corrosion issues. When i replace these part i will make them out or 316 ss instead of mild steel, but i also want to apply some sort of protective coating or paint to further extend the compoents life. Can anyone suggest a certain manufacturer or a certain product that we can apply oursleves afther the installation is complete.