I would like to know the difference in corrosivity e.q. what is more corrosive. Gas or liquid H2SO4 of high percentage (between 94 and 98 %) and operating at 50 degree celcius with a maximum of 140 degree celcius.

I would like to use this information to place a sample of some metal in the tank to calculate the corrosion rate.
 
Replies continue below

Recommended for you

It doesn't depend on the metal, it depends on the presence of liquid as strider6 said. I can't set up a viable galvanic cell without an electrolyte and gas is not an electrolyte.