Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

corrision of 2205 in concentrated salt soultion

Status
Not open for further replies.

Jtgevoc

Chemical
Joined
Dec 21, 2013
Messages
2
Location
US
Thinking of building a large evaporator to concentrate salt solutions to 25% +/-.
Planning to use 2205 tubing and contact surfaces. Vapor surfaces will be 316L

Any experience?

Thanks Jtgevoc

 
None that worked. If it is absolutely deaerated and it is cold then it might work.
I can't see 316 working if any liquid contacts it at all.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Thanks Ed,
Probably run seven effects forward flow evaporator, single pass.
If my first effect is at 100 degree C at 3% salt, will the 2205 work?
(I assume this will be the most severe condition).

The last effect will be at about 50 degrees C and 25% concentration.

I can build the entire evaporator out of 2205

Thanks JTGVOC
 