Thanks Ed,
Probably run seven effects forward flow evaporator, single pass.
If my first effect is at 100 degree C at 3% salt, will the 2205 work?
(I assume this will be the most severe condition).
The last effect will be at about 50 degrees C and 25% concentration.
I can build the entire evaporator out of 2205
Thanks JTGVOC