Hi,

Everyone can guide to correct for rubber membrane in CU triaxial test. The diameter specimen is 38mm, height to diameter ratio is 2. The thickness rubber membranes is 0.012''. I don't know to choose Young’s modulus suitable value.

Thanks,
YP
 
Use a condom and neglect it.
 
Ron - remember that MIT or Harvard (can't remember which) actually carried out tests on the "best" rubber membranes - back in the early 1970s? Trojans came in first!
 
BigH...I remember it as well. We used them for years. Higher quality and thinner than the "scientific" membranes.
 
Dave - don't tell me you reuse 'em!! Won't work so well with the end cut off!
 
Is that why I have 14 kids?





(Really only two.)
 
The lab techs always complain when they have to use the used ones!![lol]

Dave...I thought you would have figured it out after about #10.
 
If you're testing very soft or sensitive clays, it can be important.

From my graduate lab class:

Membrane resistance (N) = -pi*initial membrane diameter* thickness * 140 N/cm^2 * (axial strain +0.66*volumetric strain)

Volumetric strain is 0 for undrained shear
 
Hi, GeotechinTraining

Your formula is very good. But this is your experiential lab. Where is the formula refer? Book or paper names?

TY
 
You could check BS1377:Part 8, there is a short paragraphy about membrane correction.
 