Copper oxidation malachite prevention

Status
Not open for further replies.

Bhavindaya

Chemical
Joined
Jul 2, 2014
Messages
1
Location
ZA
How does one prevent copper oxidation during soldering process?
How does one prevent malachite formation during soldering copper pipes?
 
Flux. Prevents formation to some degree, but more importantly dissolves away any oxide that forms to keep metal surfaces clean at the point being soldered.
 