Can exfoliation alter the metal composition in copper nickel tubing?
 
Replies continue below

Recommended for you

Denickelification can appear similar to exfoliation.
It's been reported for 70Cu-30Ni (C71500) at temperatures over 100oC in low-flow conditions, and in high local temperature gradients.
ASM Handbook vol. 13 Corrosion pp. 130-133.

 