Dear all,

I am trying to define a top of the line system to handle my virgin resin and regrind, but can just think of wittmann's pneumatic conveying system. Basically I need to handle PE, PP and PC. Do you know of any other good company I could browse for a good conveying system?

Thanks for your help in advanced,

Regards,
 
Replies continue below

Recommended for you


Your location on the planet is?.....


Cheers


Harry
 
Try Consolidated Ultrasonics.

For PC you need to consider the moisture that might transfer from the air to the polymer and how you might minimise this.

Also, PC will be abrasive on the outside of the bends in the line.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor