Hello,

I am looking for a conversion table (or formula) on the internet for Shore hardness values into BS softness values.
Can anyone help me for the right site?

Thank you.

Chris
 
Replies continue below

Recommended for you

There are no dependenses for all types of materials. That dependence can be exist only in frameworks of one type of rubber. Also there are not dependence between shore hardness D, A, O and so on.
 
Hello,
I have a conversion table to convert BSS (BS 2782) to Shore A (15 sec, ASTM 2240-68) which I picked up at a trade fair from the stall of a company called PORTEX LIMITED, which is a major PVC converter in England. I am sure they have an internet address, so you can contact them. If not, give me your Fax-No and I can fax the table to you.
 
Hello,

Does anyone know where I can purchase siliconised PVC from, and possibly provide some information of the process.

p.s. Gambro, Could you please send me the conversion table you mentioned above. 01443 474222

thanks
Jenks
 
Hi Jenks,
I tried to FAX you but it didn't work, probably because we don't live in the same country. Please tell me which country you live in or send me your country code so I can try again.
 
Hello Gambro,

I tried to contact Portex. But is is very difficult to get the right person.
Can you fax the table, please?
Fax. no +31 20 6379535.

Thanks
 
Hi Jenks,
In your scramble, did you happen upon a conversion table for UHMW hardness values? I would like to apply the formulas for bearing stress and depths of maximum stress but have the UHMW hardness in Rockwell R only? Did you come across a conversion from Rockwell R to Brinell?