Guest
Please I can't convert the nuance of this Materiel (A48C3S). This nuance is in old designation AFNOR and i want to convert at ASTM code.
thanks...
 
I TOO WOULD LIKE TO KNOW THE ASTM SPECIFICATION FOR Z30C13 AFNOR SPECIFICIED METAL. THE LINK WAS NOT HELPFUL. CAN ANYONE GUIDE ME?
 
This alloy is a steel casting grade with the following composition:

C = 0.25-0.35
Si = 1.00 max
Mn = 1.00 max
Cr = 13-15

I am not that familiar with this type of steel casting alloy, so hopefully someone more knowledgeable will respond with an equivalent ASTM standard.
 