what's happening, guys?
i have a rather annoying issue to deal with. i am trying to selectively solder onto a completely gold metallized surface with AgSn or SAC solder. I have tried all different kinds of solder masks and tapes, but the adhesives breakdown at these RoHS reflow temps. Aside from machining the gold after metallization to stop flow, what else could I try?
I am also trying to make this solder as flat as possible (thickness between 100um and 150um).
any input is appreciated.
i have a rather annoying issue to deal with. i am trying to selectively solder onto a completely gold metallized surface with AgSn or SAC solder. I have tried all different kinds of solder masks and tapes, but the adhesives breakdown at these RoHS reflow temps. Aside from machining the gold after metallization to stop flow, what else could I try?
I am also trying to make this solder as flat as possible (thickness between 100um and 150um).
any input is appreciated.