is it possible to measure the temperature of continuous stream of cast iron from pressurized pouring furnace spout with a non contact IR pyrometer? The accuracy requirement is 5C (plus minus)

If yes which sensor should i use? Which company?. Which product?

Any help would be greatly appreciated.

It is a miracle that curiosity survives formal education.[Albert Einstein]
 
The temperature can certainly be measured. I am not sure if the accuracy you want can truly be attained, since it depends on both the instrument and knowledge of the conditions and properties. I suspect you can get quite close.
Jack

Jack M. Kleinfeld, P.E. Kleinfeld Technical Services, Inc.
Infrared Thermography, Finite Element Analysis, Process Engineering
 
You probably want to look at either optical thermocouples.

Or some other proprietary system.

Non contact thermocouples are really pretty good. They are little cylinders that have an optical window and two wires that are whatever T/C material they are mimicking. This allows you to hook them to any T/C reading, displaying, controlling, or logging device.

Examples:

Keith Cress