Construction of concrete cylinder curing rooms

Status
Not open for further replies.

NVizion

Structural
Jun 2, 2005
1
I was informed by my Geotechnical engineer that his curing room needs to stay at 100% humidity at all times. I am looking for information on how these rooms are commonly constructed. It seems that cmu walls are common however it seems to me that this is excessive and it doesn't answer the question about how to construct the ceiling. Please help.
 
Replies continue below

Recommended for you

NVizion

It depends on what curing regime/material/testing method etc you want to follow.

It has become appallingly obvious that our technology has exceeded our humanity
- Albert Einstein
 
Our moisture room has CMU walls with pre-cast concrete ceiling all coated with water proofing. The humidity level is maintained with an air compressor and a water line (atomized water). We go through roughly 250 cylinders a day.

Techmaximus
 