HI everyone ,

I would be really grateful if an expert in chemical anchors can answer my question.

I use Fischer vinyl ester hybrid mortar- FIS V plus 300 T. I used M8 bolt/ anchor in a 8 cm deep hole with sufficient mortar. The curing time is about 45 min according to manual. After about 2 hours without applying torque i applied about 100 kg downward tension and the anchor was stable. Around 30 min after that i used a nut to remove some left over mortar on the anchor threads and when i try to remove the struck nut with about 1 to 2 Nm torque the anchor was spinning freely. I was not able to remove nut with hand so i used pliers to hold the anchor and then removed the nut. After about 1 hour i inserted the fixture , washer and bolt and tightened to 10 Nm. To my surprise the anchor was tightened and i heard click from the torque machine. I thought i stripped the bond between the anchor threads and the resin around it. I looked on the internet but cant find any info. AI studio says anchor or bond is not damaged and said i just caused torsional rotation, but i dont trust the answer. Is my anchor really safe just because it tightened at 10 Nm torque ?
 
Vinyl ester has high shrinkage upon cure and is not a great adhesive. I would guess that the mortar lost its bond to the anchor, but not the bolt. The threads are still holding. When you threaded on the nut it could not screw the anchor any further into a blind hole, but you could unscrew the anchor. This should not affect the anchor strength significantly.
 