Hi guys,

I have been trying to measure the hardness of materials using the Japanese Micro-hardness tester MHT-1,and I have found that the machine is giving out false answers and also its calibration is not the same 700HV.

Any help to this problem is welcomed..
 
Replies continue below

Recommended for you

It would appear that the instrument is out of calibration. Contact the manufacturer and determine whether they will need to recalibrate it.

 