Mar 14, 2002 #1 jcole Mechanical Joined May 18, 1999 Messages 6 Location CA I require an epoxy with the following specs: 1. room temp or relatively low temp cure 2. electrically conductive 3. passes flammability and toxicity ratings on the MAPTIS database Does anyone know of such a product? Thanks,
I require an epoxy with the following specs: 1. room temp or relatively low temp cure 2. electrically conductive 3. passes flammability and toxicity ratings on the MAPTIS database Does anyone know of such a product? Thanks,
Mar 26, 2002 #2 iane Industrial Joined Mar 26, 2002 Messages 1 Location AU try Sauereisen Cements, Pittsburgh, they have some conductive epoxies Upvote 0 Downvote
Jul 18, 2002 #3 sandysailor Marine/Ocean Joined Jul 18, 2002 Messages 2 Location US coductivety can be acheived with the diletric addatives . temperature range cure can be modified to suit by hardener. Low toxity but i am not clear on these requirements. Mas Epoxies is great source ! Upvote 0 Downvote
coductivety can be acheived with the diletric addatives . temperature range cure can be modified to suit by hardener. Low toxity but i am not clear on these requirements. Mas Epoxies is great source !
Aug 13, 2002 #4 Gazevs Electrical Joined Aug 13, 2002 Messages 2 Location AU I need a conductive epoxy similar to (but much cheaper)than silver loaded epoxy by circuitworks. Is there an additive I can use for a standard epoxy? Something with good electrical properties, a copper, nickel or Al base. Thanks. Gary Upvote 0 Downvote
I need a conductive epoxy similar to (but much cheaper)than silver loaded epoxy by circuitworks. Is there an additive I can use for a standard epoxy? Something with good electrical properties, a copper, nickel or Al base. Thanks. Gary