Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JAE on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Concrete Testing Procedure

Status
Not open for further replies.

dik

Structural
Joined
Apr 13, 2001
Messages
26,109
Location
CA
A copy of Concrete Testing Procedure is attached for any comments or additions.

Dik
 
Those seem to be the routine controls to determine the mix design and verification that the mix as sampled after arrival is within the guidelines to match the design mix.

A testing laboratory can easily take the cylinder samples, set up site curing, transport them properly to the testing location, complete the curing to test for 2, 7, 14, 28 day and later testing specified. prepare the sample, break the cylinders and prepare reports.

Combining the sampling, site sample control, transportation and testing will put everything under one umbrella, as far as responsibility if the owner chooses this approach.

Adding extra materials (water, admix, etc. changes everything and places more responsibility on the site inspection and contractor. The cost of this responsibility must be recognized.

After that, it up the on-site materials inspector (whoever he works for), to verify that the concrete placement, finishing and site curing are done according to the specifications.

Dick

Engineer and international traveler interested in construction techniques, problems and proper design.
 
Thanks, Dick... any glaring errors?

Dik (the shorter one).
 