I've been getting reports in on concrete break strengths for a project. The majority of results of 7 day and 28 day strengths have seemed suspicious. Today, I received a report of 2 sets of cylinder breaks. The 7 day was 4,950 and 4,990 psi, respectively. The 28 day strengths are 5,010, 5,020, and 5,060 for set one, and 5,130, 5,200, and 5,090 for set two.
Has anyone heard of only a difference in 100 psi for 7 day and 28 day strengths? This concrete was normal weight, no special type of cement or curing admixtures used. Similarly, on another report, I saw 7 day breaks at 3,100 psi and 28 day breaks at 3,200 psi.
I'm starting to think the testing lab is yanking my chain here.
Has anyone heard of only a difference in 100 psi for 7 day and 28 day strengths? This concrete was normal weight, no special type of cement or curing admixtures used. Similarly, on another report, I saw 7 day breaks at 3,100 psi and 28 day breaks at 3,200 psi.
I'm starting to think the testing lab is yanking my chain here.