hi guys...
just wanna ask : is the hammer test results, say an average of 3500psi corresponds to 3500psi compressive strength of the concrete structure?
we conducted the rebound hammer test for an RC wall with a specified compressive strength of 3500psi @ 28days...the age of concrete is about 120days. base on the results,we are getting about 4130psi...
was the average test result in compliance to the parameter or specified strength?
thank you for any advise and insights...
just wanna ask : is the hammer test results, say an average of 3500psi corresponds to 3500psi compressive strength of the concrete structure?
we conducted the rebound hammer test for an RC wall with a specified compressive strength of 3500psi @ 28days...the age of concrete is about 120days. base on the results,we are getting about 4130psi...
was the average test result in compliance to the parameter or specified strength?
thank you for any advise and insights...