Is there a section or table in ACI that shows the slump limits? I would appreciate it.
 
See ACI 211 Table 6.3.1 "Recommended Slumps for Various Types of Construction" and ACI 117 Section 2.5.1.

Greg
 
Once a recommended slump has been selected and specified, the limits of the delivered slump range are then defined in ASTM C94, paragraph 6.
 