Feb 23, 2010 #1 engr567 Structural Joined Aug 21, 2009 Messages 96 Is there a section or table in ACI that shows the slump limits? I would appreciate it.
Feb 23, 2010 #2 conceng Materials Joined Jan 27, 2003 Messages 82 Location US See ACI 211 Table 6.3.1 "Recommended Slumps for Various Types of Construction" and ACI 117 Section 2.5.1. Greg Upvote 0 Downvote
See ACI 211 Table 6.3.1 "Recommended Slumps for Various Types of Construction" and ACI 117 Section 2.5.1. Greg
Feb 24, 2010 #3 Ron Structural Joined Sep 24, 1999 Messages 16,336 Location US Once a recommended slump has been selected and specified, the limits of the delivered slump range are then defined in ASTM C94, paragraph 6. Upvote 0 Downvote
Once a recommended slump has been selected and specified, the limits of the delivered slump range are then defined in ASTM C94, paragraph 6.