At the City i work for, we have used the fiber mesh on two subdivisions. These subdivision are both private streets, which made them good testing grounds. The older one is 1.5 years with the fiber mesh, and so far it seems to be a good product.
I just had a contractor working on another subdivision, one where the road will be PUBLIC, ask to use the fiber mesh.
Since this will be a public road, I was wondering if any one has any input on the fiber vs. mesh as to which is the better product. since our experience is only a few years old, I dont know that Im comfortable putting it into OUR roads.
From what i can see, the contractor is the only one to gain on this as the fiber is cheaper and easier to install than the wire. Id rather not save the contractor money if fiber is inferior to wire.
Im really looking for experience on this one. Has anyone had the fiber in the ground for longer than a few years? This is NE Ohio weather FYI. Thanks for the input!
I just had a contractor working on another subdivision, one where the road will be PUBLIC, ask to use the fiber mesh.
Since this will be a public road, I was wondering if any one has any input on the fiber vs. mesh as to which is the better product. since our experience is only a few years old, I dont know that Im comfortable putting it into OUR roads.
From what i can see, the contractor is the only one to gain on this as the fiber is cheaper and easier to install than the wire. Id rather not save the contractor money if fiber is inferior to wire.
Im really looking for experience on this one. Has anyone had the fiber in the ground for longer than a few years? This is NE Ohio weather FYI. Thanks for the input!