Concrete Creep Coefficient

Status
Not open for further replies.

NTCONLINE

Structural
Sep 29, 2012
34
What is the normal range for concrete creep coefficient (sometimes called creep factor) as defined in EC2 Clause 7.4.3?
 
Replies continue below

Recommended for you

Not sure about EC2 but below are the AS3600 values.

The long term creep coefficient is just the basic coefficient multiplied by the final coefficient.

4_zyyosv.jpg


1_b8zqrh.jpg


2_tyymy8.jpg


3_umeldf.jpg
 
Interesting the difference between the creep values.

Is there a main reason why AS3600 can be almost double the value of EC2?



 
Trenno,
I guess it could mainly be due to the local aggregates ?

I had a look at the AS3600 page 40, there is a factor dependent on the hypothesis thickness,
which seems significant.

If I design a 1-m width of a floor slab, should I use the full perimeter of the slab ? or just should use the sides which expose to the atmosphere (i.g. only top and bottom for calculation of perimeter "u") ?
 