Dec 30, 2002 #1 josephde Civil/Environmental Joined Dec 30, 2002 Messages 2 Location US On a new (4 months old slab) pre-stressed conrete slab, when is a crack a sign of structure failure on the slab and should need an special attention?
On a new (4 months old slab) pre-stressed conrete slab, when is a crack a sign of structure failure on the slab and should need an special attention?
Jan 6, 2003 #2 PaulEmil Civil/Environmental Joined Sep 16, 2002 Messages 6 Location US Was the cincrete slab pre-stressed in both directions?? Also, where did the crack occur? was it parallel to a line of prestreessing cable?? Upvote 0 Downvote
Was the cincrete slab pre-stressed in both directions?? Also, where did the crack occur? was it parallel to a line of prestreessing cable??
Jan 7, 2003 Thread starter #3 josephde Civil/Environmental Joined Dec 30, 2002 Messages 2 Location US The concrete, I believe, was pre-stressed on both directions. The a crack occurs parallel to the cable and started from a corner and the other one from the edge and mid of the slab. Upvote 0 Downvote
The concrete, I believe, was pre-stressed on both directions. The a crack occurs parallel to the cable and started from a corner and the other one from the edge and mid of the slab.