I've been asked to propose a solution to a concrete cracking problem. A pile-supported concrete floodwall, about 9' high, was constructed around a site. To provide a working surface, the contractor had cast a 9" pad along the footprint with no joints. Of course the floodwall has joints at 50' or so, and cracks have formed in the working surface at each joint. I'm looking at how (or whether) to repair the cracks, the main concern is that the occasional water infiltration will allow erosion beneath the wall, especially since the foundation is fairly recent fill.
I'm thinking drill diagonally into the cracks and inject a poly-type sealant. Any thoughts?
I'm thinking drill diagonally into the cracks and inject a poly-type sealant. Any thoughts?