Was hoping for an explanation for a test beam calculation ... Have been beating my head against this for the last few hours and not coming up with the same number from a previous correct sheet .
The formula is R = 1.05 Pl / bd^2
P = Maximum applied load - 350
l= span length in " 18 "
b = width in" 5.88 "
d = depth " 6.04"
This formula should also achieve the same result but not making sense to me .
CF = Exact / Actual
R= 1.05( psi )CF / 145 .
Any help would be greatly appreciated ....
Thanks
Was hoping for an explanation for a test beam calculation ... Have been beating my head against this for the last few hours and not coming up with the same number from a previous correct sheet .
The formula is R = 1.05 Pl / bd^2
P = Maximum applied load - 350
l= span length in " 18 "
b = width in" 5.88 "
d = depth " 6.04"
This formula should also achieve the same result but not making sense to me .
CF = Exact / Actual
R= 1.05( psi )CF / 145 .
Any help would be greatly appreciated ....