BHmax = 52 MGOe
Br = 14.5kG
Hci = 11.0 kOe
Hc = 10.6 kOe
U0 = .000001256636
I am working on a project with coils and electromagnets and the information above is from a B/H chart and the values for magnetic flux density and coercive force are for neodymium N5211 metal. I know that Br is the remaneant flux density of the metal and I'm not sure which if is that the number I should use to compute the permeability(mu)and also not sure which number for coerce force I need to use to get the correct magnitude, so here goes.
u=B/H=14.5/11.0(Hci)=1.318181818181818
u=B/H=14.5/10.6(Hc) =1.367924528301887
Relative Permeability(ur)=u/u0=1.31818/.000001256636=1048975.20045582 for Hci and
1088560.251337698 for Hc.
First is the numbers I used to compute the permeability the correct numbers to use to start with to calculate permeability of N5211?
Which numbers would be the correct numbers to plug into an equation to get the correct magnitutde, Hci or Hc? Any help from anyone would be greatly appreciated.
Thanks
neferkamichael
BHmax = 52 MGOe
Br = 14.5kG
Hci = 11.0 kOe
Hc = 10.6 kOe
U0 = .000001256636
I am working on a project with coils and electromagnets and the information above is from a B/H chart and the values for magnetic flux density and coercive force are for neodymium N5211 metal. I know that Br is the remaneant flux density of the metal and I'm not sure which if is that the number I should use to compute the permeability(mu)and also not sure which number for coerce force I need to use to get the correct magnitude, so here goes.
u=B/H=14.5/11.0(Hci)=1.318181818181818
u=B/H=14.5/10.6(Hc) =1.367924528301887
Relative Permeability(ur)=u/u0=1.31818/.000001256636=1048975.20045582 for Hci and
1088560.251337698 for Hc.
First is the numbers I used to compute the permeability the correct numbers to use to start with to calculate permeability of N5211?
Which numbers would be the correct numbers to plug into an equation to get the correct magnitutde, Hci or Hc? Any help from anyone would be greatly appreciated.
Thanks
neferkamichael