We manufacture a part approximately 3 mm thick (obtaine by fine blanking) with 3 zones surface hardened (high frequency treatment) for years.
We thought that this kind of treatment lead gave always a compressive state of the heat treated zones until we carried out stress measurements because of micro-crack problems.
We are now very surprise by the results : the presence of a layer of tension stress of about 10 µm depth.
Could anyone bring us his experience.... Thanks