Magnets that are believed to be NdFeB Grade N48 with nickel plating were sent to an independent laboratory to be analyzed for material content. The resulting chemistry (sans plating) shows the composition to be:
Fe 67.1%
Nd 31.9%
B 1%
Given the above properties, is there any way to determine the Grade of this material (N48, N50, N50H, N48UH, etc. etc.)? I don’t believe that there is, however I’m being asked and before I give my less than optimistic response I’d like to hear from the experts.
[link ]
[/url]
Fe 67.1%
Nd 31.9%
B 1%
Given the above properties, is there any way to determine the Grade of this material (N48, N50, N50H, N48UH, etc. etc.)? I don’t believe that there is, however I’m being asked and before I give my less than optimistic response I’d like to hear from the experts.
[link ]