I am studying carbon fiber laminate for structural loads thro FEA. I use hypermesh/optistruct (same as Nastran keyword format) to analyze the FE models. My model contains 64 lamina with repeating material directions. (The laminate has 8 quasi-isotropic lamina assemblies. Each quasi-isotropic lamina assembly has 8 layers/lamina with material angle in 0, 45, 90,-45, -45, 90, 45, 0 as the stacking sequence) I use Pcomp and Mat8 combination. My material has failure strain values to capture the failure index based on maximum strain theory.
As the post processing becomes laborious with 64 laminas, I tried to use SMEAR property in PCOMP card. I used COMPRO program to generate the material property for quasi isotropic laminate based on 8 layers with above mentioned stacking sequence. Then I reduced the number of layers in my FE model, from 64 to 8 and I referenced smeared material property for each layer.
Now my doubt is
1) Should I turn on smear field in Pcomp card? Or does not matter?
2) What angle I should use for each layer? Does the angle matter in this situation as the E1=E2 in the smeared property?
3) My biggest doubt is interlaminar shear stress (SB) in PCOMP card. When I did my first analysis (with individual 64 layer), I used the shear strength of epoxy resin for SB value. (However I did not model separate bonding layer between carbon fiber layers, as bonding layers are very thin, may be 0.001 inch due to our high pressure compaction. Also, if I model bond layer it will become 128 layers, instead of 64 layers.). When I used the same SB value in second analysis (8 layers with smeared material properties), the results are completely different with first analysis particularly bond failure index. It is so higher than the first analysis. I do not know how to fix this. Gurus, help me to fix this and how to perform smeared analysis.
Thank you.
As the post processing becomes laborious with 64 laminas, I tried to use SMEAR property in PCOMP card. I used COMPRO program to generate the material property for quasi isotropic laminate based on 8 layers with above mentioned stacking sequence. Then I reduced the number of layers in my FE model, from 64 to 8 and I referenced smeared material property for each layer.
Now my doubt is
1) Should I turn on smear field in Pcomp card? Or does not matter?
2) What angle I should use for each layer? Does the angle matter in this situation as the E1=E2 in the smeared property?
3) My biggest doubt is interlaminar shear stress (SB) in PCOMP card. When I did my first analysis (with individual 64 layer), I used the shear strength of epoxy resin for SB value. (However I did not model separate bonding layer between carbon fiber layers, as bonding layers are very thin, may be 0.001 inch due to our high pressure compaction. Also, if I model bond layer it will become 128 layers, instead of 64 layers.). When I used the same SB value in second analysis (8 layers with smeared material properties), the results are completely different with first analysis particularly bond failure index. It is so higher than the first analysis. I do not know how to fix this. Gurus, help me to fix this and how to perform smeared analysis.
Thank you.