Dear Sir,
We are an incinerator maker in Indonesia. The flue gas outlet from incinerator will be about 900 deg C. To cool the flue gas, we make two pass gas cooler with water inside the shell, and hundreds of fire tube. The construction is same like a fire tube boiler diameter 63.5 x 2.9 mm thk with 175 tubes in the first pass and 100 tubes in the second pass. The outlet temperature of gas will be about 180 deg C. The shell diameter is 2200 mm OD
My questions:
1. Is it mandatory to design the gas cooler as per ASME sec 1 ? or is it applicable to design the gas cooler with ASME sec VIII? Note: This is not an ASME Stamp equipment. The shell material is A516Gr70 plate and A312TP316L tubes
2. As per ASME1995 sec 1 PFT 9.1, the minimum shell thickness with diameter over 72 “ is ½”. Is it still applicable to the latest edition?
3. What happen if the thickness selected 10 mm only?
4. What is the strength value of both above material as per the latest edition?

Thank you very much for your suggestion.

With best regards,,

Calvin barus

 
Section I will not permit the use of 316 SS material in heat transfer components in contact with water, to avoid chloride stress corrosion cracking. Section VIII might allow this , and normally when a boiler mfr wants to use 316 SS for an economizer he would use section VIII. Such chloride stress cracking cannot occur if the metal temperature can be positively guaranteed not to exceed 300F / 148 C, and you may be close to that in some areas.

I think certain details need to be worked out in order to avoid including the component in the section I scope as defined in fig PG-58.3.1 . See U-1(g), UG-16(b)(3), UG-125(b), UW-2(c), and UCS-25 of section VIII and part PFH of section I, and code case 1855 and PG-112.2.6
 
OOPs.

To correct some wrong info I submitted above. The chloride stress corrosion cracking ( SCC) can occur below 300F/ 148 C, so I think that one needs to review the metal selection and water quality with the issue of SCC in mind.
 
Design your incinerator per ASME power boiler code I or heating boiler code IV. Your selection will be bases on MAWP. I consider your installation as fired PV's.
 