Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Combining Nozzle Reinforcement Plate - API650 Para 5.7.2.9 vs Fig 5.6

Status
Not open for further replies.

wailunwu

Mechanical
Joined
Jun 25, 2013
Messages
33
Location
CA
Para 5.7.2.9 states the requirement between the outer edges of the reinforcing plate fillet welds (closer than 8w or 6in). This is the same requirement for fig 5.6, column E, with shell thickness t > 0.5, as welded condition.

My question is:
Does Para 5.7.2.9 only apply to t > 0.5in as welded condition? How do combine reinforcement for t<0.5in, as welded condition?


Please Advise,

Thanks
Alan
 
The way it reads it applies to all shell thicknesses. But you raise a good question and it deserves a technical inquiry.
 