Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Column Lap Length and lapping Zone

Status
Not open for further replies.

Sheikhmoeed

Civil/Environmental
Dec 7, 2016
3
Hello,
At my site, i am facing an issue regarding lap length of column. First, all the laps are just on the slab(at starter point) and second most important, my remaining lap that is left behind for lapping of further column is just 36" and we are using #8 bar.
So, is it ok to provide 36" lap just at the starter zone? if not, then what to do?
please share your opinion.
 
Replies continue below

Recommended for you

What concrete code or specification are you under? ACI? Eurocode? Other?



Check out Eng-Tips Forum's Policies here:
faq731-376
 
With the exception of some high seismic situations, it's pretty normal to lap your column bars at the slab level. Easy to build. As far as the lap length goes, you need to provide a lap length that will develop your bars for whatever tension or compression forces you expect to see in the joint. Most designers will simply specify a full lap splice for simplicity.

I like to debate structural engineering theory -- a lot. If I challenge you on something, know that I'm doing so because I respect your opinion enough to either change it or adopt it.
 
So, in your opinion, what should be the lap length for 25mm dia bar in column?
Is 3feet lap length is enough or not?
 
The lap length depends on whether it is a compression only slice or a splice that has tension. Several factor such as cover and concrete strength can affect the required length of tension splices. The engineer responsible for the design should answer this question.
 