The problem is that we have large petroleum tanks ( 15000 -50000 ) cubic meter capacity
some tanks'shells are damaged ( corrosion , bullets ...) ,the tanks are in service and we have to repair the damaged shell !!!!!
I read about a material ( paste ) that can be but on the hole and it fill the hole..I don't know where or how to get it
and the more important is it approved according to the standards