Cold Rolled Steel

Status
Not open for further replies.

chrisakel

Mechanical
Jun 3, 2003
2
How can tool wear be reduced on cold rolled steel?
 
Replies continue below

Recommended for you

Better lubrication....

Rougher surface.....

nick


Nick
I love materials science!
 
In addition to NickE's comments, softer temper cold rolled steels might be be used, provided the end product strength requirements are met.

 