Thanks for the information.
My original post was lacking some information.
We have two Cr-½Mo Coke drums that were installed in 1979. External cracking in the bottom section of the drums were removed by grinding/weld repair, however PWHT resulted in new cracks. These new cracks were removed without weld repair. At the next outage, the cracking returned, with the same grind/weld/PWHT/crack removal sequence.
I am considering two options for the future of our Coke drums.
1. Replace the bottom 1/3 of the drums.
2. Replace the drums completely.
Obviously, cost is the main driver for considering option 1. I know that many refineries have replaced Coke drums due to cracking/bulging in the past 10 years.
I would like to know if anyone has replaced the bottom section of the drum and what sort of issues did they encounter (additional cracking above the new section, need to replace top section after a period of time, etc.). Alternatively, it would be helpful if anyone has a good reason to stay away from a partial replacement.
I appreciate any help that the group can provide.
Thanks,
John Leroux