Does anyone have any data for the coefficient of thermal expansion of NBR? The durometer would be ~ 75 Shore A.
 
Replies continue below

Recommended for you

Per Machine Design Handbook, CTE is:
39 x 10-5 per degree F (cubic).
 
MIL-HDBK-149B lists it as 112 [·] 10-6 K-1

Regards,

Cory