Coefficient of friction between steel and concrete??

Status
Not open for further replies.

KeithW62

Mechanical
Jun 18, 2002
1
Can anyone tell me what the coefficient of friction between steel and concrete is. Many thanks in advance for this information.
-Keith
 
Replies continue below

Recommended for you

The only figure that I have seen documented is 0.5 (specified in the Australian Bridge Desigb Code).

I have used that (with a reasonable safety factor) for designing temporary support brackets stressed onto bridge piers etc, and so far it has worked for me.

 
ACI 318 Section 11.7.4.3 gives the coefficient of friction for several conditions.
 