Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

CODE CASE 2418 for S32101 Material

Status
Not open for further replies.

ruthi

Mechanical
Joined
Mar 8, 2010
Messages
9
Location
US
Hi All,
Can anyone provide a copy of code case 2418 or suggest where I could find one? Is it true that ASME provides code cases for free to all the code users? Did anyone experience strength welding S32101 tubes to c/stl clad with S32101 tubesheet? This is the first time we are trying to use this material and have no clue how to/where to start from.

Thanks in advance for your response.
 
Yes, ASME Code Committee members get code case information free.

There have been some real problems trying to weld lean duplex tubes directly to carbon steel tube sheets. Recommendations are to use a high nickel filler metal to get good results. However, provided your clad is thick enough that the entire strength weld is fully encompassed in the clad and does not melt into the carbon steel backer, you should have no problem making the weld. Typical filler metal is ER2209. You can use weld procedures typically used for Alloy 2205.
 
Thanks for the info Mike. I am assuming this one is published and is in use.Is there any quicker way to get this code case 2418?

Thanks again.
Rathi
 
The Code Case defines the chemistry, minimum mechanical properties, design allowable stresses at temperature and minimum solution annealing temperature. It does not tell you how to weld it. Per (d)of the Code Case "Seperate welding procedure qualifications and performance qualifications shall be conducted as prescribed in Section IX."

MikeMet has provided you a recommended filler metal. Nickel base alloy fillers (E/ERNiCrMo-X) could also be used. Limit Interpass Temperature.

 
Stanweld:
I am running a design using S32101 wld tubes and c/stl tubesheet with 5/16" tk S32101 overlay. Tubes are strength welded to tubesheet. Current code does not include S32101 material and the only way I can get the stress values and other required data is through that code case.
Thank you for your response. I will go through section IX for welding info.
 
ruthi,
Assuming that the expchanger will be U stamped, you will need to obtain a copy of the Code Case. If it is not stamped, please provide the design temperature and thickness.

 
Design temp on tubeside is 150 Deg F, we are using 3/4" OD x 0.065(AW)SA-789-S32101 wld tubes.
 
Design allowable is 28.9 ksi for t less than or equal to 0.187" (5 mm), 26.9 ksi fot t > 0.187" (5 mm). at the design temp. Maximum permitted design temp is 600F (325C).

 