Jul 7, 2008 #1 FYS Petroleum Joined Jun 24, 2008 Messages 22 Location AE Hi, Please can you advise a coating for 316 Stainless Steel (Instrument Unit - normal Temperature) in immersed/buried condition (High Water Table.