I am repairing a concrete slab and containment walls that can be exposed to bleach pH = 10-12. The slab and walls are for secondary containment and would only experience short term exposure to the bleach, less than 72 hours. Has anyone had good experience with a coating for this application?
 
Replies continue below

Recommended for you

I'd be looking for an epdm coating compound, there are products made for lining concrete tanks and ponds that should work.
 
Agree with Ron. Read the PDS, then call Carboline with any questions you have. Observe all safety/personal protection requirements.
 
Check MSDS sheets very carefully... material can be carcinogenic.



Dik
 